ABSTRACT:
Metal treating compositions, containing chromic acid and pulverulent zinc, and which find particular utility in the coating of metal substrates prior to painting, now exhibit extended bath stability through pH adjustment. The key to the adjustment is not in the final bath makeup. Rather, the adjustment is made during preparation of a precursor component containing chromic acid. Such component of adjusted pH may then be blended with additional composition ingredients including the pulverulent zinc to form a bath of excellent stability, e.g., extended freedom from gelation.
REFERENCES:
patent: 3553034 (1971-01-01), Harvey et al.
patent: 3671331 (1972-06-01), Malken et al.
patent: 3687738 (1972-08-01), Malken
patent: 3687739 (1972-08-01), Kennedy et al.
patent: 3849141 (1974-11-01), Palm et al.
DE Ridder Jon A.
Gunn Walter H.
Kennedy Alexander W.
Diamond Shamrock Corporation
Freer John J.
Kendall Ralph S.
Wolfe, Jr. Charles R.
LandOfFree
Metal treating compositions of adjusted pH does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Metal treating compositions of adjusted pH, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Metal treating compositions of adjusted pH will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1723919