Metal repair tape for superalloys

Stock material or miscellaneous articles – All metal or with adjacent metals – Having metal particles

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

428547, 428556, 428557, 428560, 428564, 428565, 2940209, 2940216, B22F 702

Patent

active

055231691

ABSTRACT:
A base metal repair tape includes a first layer formed from powdered base metal bonded together by fibrillated polytetrafluoroethylene and a second layer comprising a brazing alloy bonded together by fibrillated polytetrafluoroethylene. This is used to repair base metal by placing the first layer on the base metal and brazing the base metal so that the brazing alloy melts and diffuses into the base metal powder bonding it to the surface of the article. This permits the braze powder to be bonded to the base metal surface with minimal distance between the base powder particles.

REFERENCES:
patent: 2808352 (1957-10-01), Coleman et al.
patent: 3293072 (1966-12-01), Doolittle et al.
patent: 3719538 (1973-03-01), Carlson et al.
patent: 3743556 (1973-07-01), Breton et al.
patent: 3759692 (1973-09-01), Zelahy
patent: 3778586 (1973-12-01), Breton et al.
patent: 3841942 (1974-10-01), Carlson et al.
patent: 3864124 (1975-02-01), Breton et al.
patent: 3876447 (1975-04-01), Lally
patent: 3917149 (1975-11-01), Breton et al.
patent: 3997447 (1976-12-01), Breton et al.
patent: 4016345 (1977-04-01), Holmes
patent: 4042747 (1977-08-01), Breton et al.
patent: 4098450 (1978-07-01), Keller et al.
patent: 4112180 (1978-09-01), Steigelman
patent: 4194040 (1980-03-01), Breton et al.
patent: 4228214 (1980-10-01), Steigelman et al.
patent: 4325754 (1982-04-01), Mizuhara et al.
patent: 4381944 (1983-05-01), Smith, Jr. et al.
patent: 4477527 (1984-10-01), Grosner
patent: 4478638 (1984-10-01), Smith, Jr. et al.
patent: 4528230 (1985-07-01), Larson
patent: 4546047 (1985-10-01), Ryan
patent: 4563329 (1986-01-01), Morishita et al.
patent: 4596746 (1986-06-01), Morishita et al.
patent: 4624860 (1986-11-01), Alber et al.
patent: 4726101 (1988-02-01), Draghi et al.
patent: 4830934 (1989-05-01), Ferrigno et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Metal repair tape for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Metal repair tape for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Metal repair tape for superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-382249

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.