ABSTRACT:
The present invention aims to provide a metal mold for glass, which needs not apply any swab in molding of glass, enabling no-swabbing glass forming. The alloy for the mold comprises by weight Cu: 10 to 80%, Al: 4 to 11%, Cr: 3 to 16%, Ni: 2 to 36%, and at least one rare earth element: 0.02 to 2.08 with the balance consisting of Fe and further comprises at least one member selected from the group consisting of Ti: Al %.times.0.5 to 2, V: Al %.times.0.2 to 1, Zr: Al %.times.0.1 to 0.3, and Nb: Al %.times.0.1 to 0.3. The alloy is gradually cooled from the solidification initiation temperature to 500.degree. C. at a cooling rate of 10.degree. C./min. The surface of the mold is coated with an Al-containing coating or roughened to an average roughness of 0.3 to 5 .mu.m. A solid lubricating film is provided in a fitting portion of the mold, or alternatively a self-lubricating solid is embedded in the fitting portion of the mold.
Akafuji Koji
Arikata Isao
Endo Michio
Hirata Mitsuji
Imamura Hiroto
Ip Sikyin
Nippon Steel Corporation
LandOfFree
Metal mold for glass forming does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Metal mold for glass forming, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Metal mold for glass forming will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-156927