ABSTRACT:
Described herein are nickel-chromium-iron maraging, gamma prime strengthened superalloys containing about 18 to 25 weight percent nickel, about 4 to 8 weight percent chromium, gamma prime forming elements such as aluminum and/or titanium, and a solid solution strengthening element, such as molybdenum. After heat treatment, which includes at least one ausaging treatment and at least one maraging treatment, a microstructure containing gamma prime phase and decomposed Fe-Ni-Cr type martensite is produced.
REFERENCES:
patent: 3199978 (1965-08-01), Brown et al.
patent: 4049431 (1977-09-01), Hagel et al.
patent: 4125260 (1978-11-01), Kanne et al.
patent: 4129462 (1978-12-01), Korenko
patent: 4172742 (1979-10-01), Rowcliffe et al.
patent: 4259126 (1981-03-01), Cole et al.
patent: 4359349 (1982-11-01), Merrick et al.
Cupp et al., Trans. Metall. Soc. of AIME, 239, pp. 1468-1472, Sep. 1967.
Metals Progress, vol. 28, pp. 99-100, Nov. 1980.
Hall et al., NASA-SP-5051, U.S. Gov't. Printing Off., p. 137, 1968.
Floreen, Metals and Materials, 2, pp. 115-128, 1968.
Metals Handbook; vol. 2, 8th Ed., pp. 255-256, 1964.
Floreen, Trans. Metall. Soc. of AIME, 236, pp. 1429-1440, Oct. 1966.
Gelles David S.
Korenko Michael K.
Thomas Larry E.
O'Keefe Veronica
Prizzi John J.
The United States of America as represented by the United States
LandOfFree
Maraging superalloys and heat treatment processes does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Maraging superalloys and heat treatment processes, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Maraging superalloys and heat treatment processes will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1012014