Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Polymers from only ethylenic monomers or processes of...
Patent
1975-04-18
1976-10-19
Holler, Alan
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Polymers from only ethylenic monomers or processes of...
526 6478, 526 82, 526 88, C08F 202, C08F 238, C08F 1002
Patent
active
039870200
ABSTRACT:
Ethylene polymers are produced at pressures between 1000 and 4000 atmospheres and temperatures of from 120.degree. to 300.degree. C in a reaction zone having an 1/d ratio of from 10:1 to 20:1 while shear forces act on the reaction mixture. The ethylene is fed continuously and radially to the reaction zone at a velocity of from 2 to 20 m/sec. The average residence time of the reaction mixture in the reaction zone is from 20 to 90 seconds. The products show a broad molecular weight distribution and are particularly advantageous for use as extruded coatings.
REFERENCES:
patent: 2897183 (1959-07-01), Christl et al.
patent: 3536693 (1970-10-01), Schrader et al.
patent: 3575950 (1971-04-01), Gleason et al.
patent: 3692763 (1972-09-01), Van Saane et al.
patent: 3756996 (1973-09-01), Pugh et al.
Gropper Hans
Oeder Dieter
Urban Friedrich
BASF - Aktiengesellschaft
Holler Alan
LandOfFree
Manufacture of ethylene polymers does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Manufacture of ethylene polymers, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Manufacture of ethylene polymers will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-101350