Making of steel component

Metal treatment – Compositions – Heat treating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148 165, 148318, 148319, C21D 174

Patent

active

047102381

ABSTRACT:
A component formed of interstitial free steel is heated in a gaseous atmosphere containing 15% by volume of a nitrogen doner, e.g. ammonia, at about 500.degree. C. to about 740.degree. C. for about 30 minutes to about 4 hours to form an epsilon iron nitride surface layer, and a layer of nitrides of trace alloying elements below the surface layer.

REFERENCES:
patent: 4496401 (1985-01-01), Dawes et al.
Harterei-Technische Mitteilungen, vol. 29, #1, 3/74, pp. 42-49.
Patents Abstracts of Japan, vol. 8, #56 (C-214), (1493), Mar. 14, 1984.
Chemical Abstracts, vol. 89, #24, Dec. 1978, p. 230, Abstract #20141d, Cols, Ohio, J. Bidlen, "Effect of Nitridation . . . ".
Chemical Abstracts, vol. 67, 1967, p. 8794, Abstract #93222v, Columbus, Ohio.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Making of steel component does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Making of steel component, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Making of steel component will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1929485

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.