Metal treatment – Stock – Magnetic
Patent
1997-09-26
2000-06-06
Zimmerman, John J.
Metal treatment
Stock
Magnetic
148304, B22F 100
Patent
active
060713577
ABSTRACT:
A metal-matrix composite of magnetostrictive powder is manufactured by dynamic compaction, such as that provided by the shock waves of an explosive, from a magnetostrictive powder in the presence of a matrix-forming metal. Under the conditions of dynamic compaction, property compromising phases between the powder and the binding metal are not formed, resulting in a composite essentially free of these phases. The composites may be formed by coating a magnetostrictive powder with a matrix-forming metal by a sputtering process and dynamically compacting the coated powder. A coated powder may also be made by sputtering a layered composite of metal-magnetostrictive material-metal, and grinding the layered composite. Metal-matrix composites may also be made by mixing the matrix-forming metal with a magnetostrictive powder and dynamically compressing the mixture. Metal-matrix composites of amorphous magnetostrictive powders may be annealed in the presence of a magnetic field.
REFERENCES:
patent: 1286965 (1918-12-01), Elmen
patent: 1292206 (1919-01-01), Woodruff
patent: 3156039 (1964-11-01), Martens
patent: 3160952 (1964-12-01), Corney et al.
patent: 3215565 (1965-11-01), Harvey
patent: 3218199 (1965-11-01), Cowan et al.
patent: 3228757 (1966-01-01), Verbraak
patent: 3445296 (1969-05-01), Hidekazu Abe et al.
patent: 3615915 (1971-10-01), Luiten et al.
patent: 3986944 (1976-10-01), Gould
patent: 4159909 (1979-07-01), Wilson
patent: 4484995 (1984-11-01), Pirich et al.
patent: 4711795 (1987-12-01), Takeuchi et al.
patent: 4814053 (1989-03-01), Shimokawato
patent: 4889607 (1989-12-01), Buschow
patent: 4906306 (1990-03-01), Araki et al.
patent: 4929320 (1990-05-01), Yamada et al.
patent: 4933025 (1990-06-01), Alson et al.
patent: 4933059 (1990-06-01), Sugawara et al.
patent: 4939041 (1990-07-01), Kabacoff et al.
patent: 4940523 (1990-07-01), Takeshima
patent: 5505903 (1996-04-01), Schrey et al.
patent: 5907105 (1999-05-01), Pinkerton et al.
F. E. Pinkerton, et al. "Magnetostricitive Composites" General Motors Corporation, Resarch and Development Center, R&D-8605, Nov. 13, 1996.
K. B. Hathaway, et al. "Magnetostrictvie Materials" MRS Bulletin, vol. XVIII, No. 4, Apr. 1993.
Guruswamy, et al. "Explosive Compaction of Metal-Matix Composites and Deuterides" Advance in Power Metallurgy, Vo. 6, Metal Powder Industies Federation, Leander, et al. Eds., (1991) (no month).
Herbst, et al. "Estimating the Effective Magnetostrictiion of a Composite: A simple Model"General Motors Corporation, Research and Development Center, R&D-8608, Nov. 25, 1996.
C. Rogers, "Intellignet Materials" Scientific American, Sep. 1995.
Guruswamy Sivaraman
Loveless Michael R.
McCarter Michael K.
Savage Jason
Sonntag James L.
Zimmerman John J.
LandOfFree
Magnetostrictive composites and process for manufacture by dynam does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Magnetostrictive composites and process for manufacture by dynam, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Magnetostrictive composites and process for manufacture by dynam will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2210465