Magnetically anisotropic R-T-B magnet

Metal treatment – Process of modifying or maintaining internal physical... – Magnetic materials

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148104, 419 11, 419 34, 419 35, H01F 102

Patent

active

051620634

ABSTRACT:
A magnetically anisotropic R-T-B magnet having crystal grains having aspect ratios of 2 or more and showing a substantially uniform maximum energy product distribution is produced by (a) rapidly quenching an alloy melt; (b) finely pulverizing the rapidly quenched alloy to provide magnetic powder; (c) mixing the magnetic powder with a carbon-containing additive; (d) coating the resulting mixture with a protective layer of a first lubricant such as BN substantially unreactive with the alloy components; (e) compressing it; (f) further coating the resulting compressed body with a second lubricant such as graphite or graphite+glass; and (g) further compressing it.

REFERENCES:
patent: 4780226 (1988-10-01), Sheets et al.
patent: 4952251 (1990-08-01), Iwasaki et al.
patent: 4978398 (1990-12-01), Iwasaki et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Magnetically anisotropic R-T-B magnet does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Magnetically anisotropic R-T-B magnet, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Magnetically anisotropic R-T-B magnet will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2290886

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.