ABSTRACT:
In a metal-in-gap magnetic head, a pair of magnetic core halves made of ferrite are arranged to oppose to each other, and metallic magnetic films are applied to each of opposing surfaces of the pair of magnetic core halves. A hard glass layer and a chromium layer are applied to a gap plane of the magnetic head as a gap layer. A gap is formed so as to abut on the chromium layers between a pair of the gap layers. The hard glass layer includes borosilicate as a main component and it has Vickers hardness of the same as that of said metallic magnetic films or less and softening temperature of 550.degree. C. or higher. Thus, a magnetic head does not generate a spacing loss when a tape slides thereon.
REFERENCES:
patent: 3458926 (1969-08-01), Maissel et al.
patent: 4048714 (1977-09-01), Huntt
patent: 4170032 (1979-10-01), Yokoyama et al.
patent: 4475137 (1984-10-01), Yasuda et al.
patent: 4948667 (1990-08-01), Mikami et al.
patent: 5001590 (1991-03-01), Saito et al.
patent: 5034273 (1991-07-01), Sakakima et al.
patent: 5155645 (1992-10-01), Shimizu et al.
J.F. Dundovic, "Magnetic-Head Relapping Techniques", Project Notes/Engineering Briefs, Journal of the Audio Engineering Society, vol. 24, No. 8, May 1976, New York, pp. 656-659.
Ashida Akihiro
Hasegawa Hiroyuki
Sawai Eisuke
Takahashi Ken
Takeda Hiromi
Matsushita Electric - Industrial Co., Ltd.
Resan Stevan A.
LandOfFree
Magnetic head does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Magnetic head, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Magnetic head will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1254804