Low tin terne coating

Coating processes – With post-treatment of coating or coating material – Gas jet or blast mechanically treats coating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

B23B 1504

Patent

active

044169205

ABSTRACT:
The application discloses a method of terne coating, and a terne coated product, wherein the tin content of the terne is substantially lower than in conventional terne, without the need for other alloying elements in substitution for tin, such as zinc, antimony, silver, and phosphorus. The tin content of the terne bath is lowered below conventional percentages, to between about 2% and about 6.5% and the terne coated product, upon emerging from the coating bath, is jet finished. Such a terne coat has improved solderability and appearance with no change in pinhole frequency. Coating weight control is easier than with a terne coat having 7% or more tin in the bath.

REFERENCES:
patent: T913003 (1973-08-01), Siple
patent: 3607366 (1971-09-01), Kurokawg
patent: 3808033 (1974-04-01), Mayhew
patent: 3819406 (1974-06-01), Tachimori
patent: 3917888 (1975-11-01), Beam

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Low tin terne coating does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low tin terne coating, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low tin terne coating will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1815058

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.