ABSTRACT:
The combination of strength and fracture toughness properties of aluminum-lithium alloys are significantly enhanced by underaging the alloys at temperatures ranging from 200.degree. F. to below 305.degree. F. for relatively long periods of time.

REFERENCES:
patent: 4840682 (1989-06-01), Curtis et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Low temperature underaging of lithium bearing alloys and method does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low temperature underaging of lithium bearing alloys and method , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low temperature underaging of lithium bearing alloys and method will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-446926

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.