Low temperature lithiation of mixed hydroxides

Chemistry of inorganic compounds – Treating mixture to obtain metal containing compound – Alkali metal

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C423S593100, C423S594400, C423S594600, C423S599000, C423S594150, C423S594190, C423S605000, C423S641000, C423S196000, C423S184000

Reexamination Certificate

active

07033555

ABSTRACT:
A low temperature contaminant limiting process for lithiating hydroxides and forming lithiated metal oxides of suitable crystalinity in-situ. M(OH)2is added to an aqueous solution of LiOH. An oxidant is introduced into the solution which is heated below about 150° C. and, if necessary, agitated. M may be selected from cobalt, nickel and manganese. The resultant LiMO2becomes crystallized in-situ and is subsequently removed.

REFERENCES:
patent: 4567031 (1986-01-01), Riley
patent: 5356731 (1994-10-01), Sitters et al.
patent: 5630993 (1997-05-01), Amatucci et al.
patent: 5891416 (1999-04-01), Yamazaki et al.
patent: 6048643 (2000-04-01), Van Ghemen et al.
patent: 6296972 (2001-10-01), Hong et al.
patent: 6399041 (2002-06-01), Ado et al.
patent: 6447739 (2002-09-01), Krynitz et al.
patent: 6589695 (2003-07-01), Kweon et al.
patent: 6949233 (2005-09-01), Kweon et al.
patent: 6960335 (2005-11-01), Singhal et al.
patent: 2001/0016284 (2001-08-01), Kweon et al.
patent: 2003/0022063 (2003-01-01), Paulsen et al.
patent: 2003/0044684 (2003-03-01), Nanamoto et al.
patent: 2004/0241547 (2004-12-01), Gao et al.
patent: 2005/0130042 (2005-06-01), Liu et al.
patent: 1357491 (2002-07-01), None
patent: 0 867 408 (1998-09-01), None
patent: WO 97/02214 (1997-01-01), None
Xiaoming et al., “Manufacture of cobalt-lithium oxide”, Chemical Abstracts Services, Columbus, Ohio, Jul. 10, 2002, XP002293225.
Holleman and Wiberg, “Lehrbuch der Anorganischen Chemie”, Berlin New York, p. 1550, line 1-32, p. 1553, line 25 & p. 1554, line 42.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Low temperature lithiation of mixed hydroxides does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low temperature lithiation of mixed hydroxides, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low temperature lithiation of mixed hydroxides will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3555630

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.