Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Ethylenically unsaturated reactant admixed with either...
Patent
1979-12-04
1981-02-17
Ziegler, J.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Ethylenically unsaturated reactant admixed with either...
525 34, 525444, 525445, C08L 6700
Patent
active
042516412
ABSTRACT:
Unsaturated polyester resin compositions that have a low shrinking property, and at the same time, an enough strength are provided. The compositions comprises (1) 30-70 parts by weight of an unsaturated polyester obtained by reactin terephthalic acid and/or isophthalic acid and one or more of unsaturated acids selected from the group consisting of maleic anhydride, maleic acid and fumaric acid, with a glycol, and having the unsaturation degree of 1.5-5.0 and the acid value of 18-40, (2) 70-30 parts by weight of .alpha.,.beta.-ethylenically unsaturated monomer, and (3) 5-30 parts by weight of an amorphous linear saturated polyester resin obtained by reacting terephthalic acid and/or isophthalic acid with a glycol component.
REFERENCES:
patent: 3489707 (1970-01-01), Fry
Arakawa Kouji
Nomaguchi Kanemasa
Hitachi Chemical Company Ltd.
Ziegler J.
LandOfFree
Low shrinkage polyester resin compositions does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low shrinkage polyester resin compositions, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low shrinkage polyester resin compositions will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2263191