Low-odor, higher molecular weight polyether polyols, a process f

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – From reactant having at least one -n=c=x group as well as...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

528 76, 528 77, 568679, 568680, C08G 1832

Patent

active

056523190

ABSTRACT:
Low-odor, higher molecular weight polyether polyols are produced by purifying the polyether polyols at temperatures of 110.degree. to 150.degree. C. and pressures of 10 to 70 hPa with the addition of 5 to 30% by weight of water, wherein the water is passed in finely divided form, with a droplet diameter of about 5 to 100 .mu., through the polyether polyols to be purified for a time of metered addition of 1 to 5 hours.

REFERENCES:
patent: 3653183 (1972-04-01), Sanders et al.
patent: 4143072 (1979-03-01), Hetzel et al.
patent: 5248794 (1993-09-01), Choppell et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Low-odor, higher molecular weight polyether polyols, a process f does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low-odor, higher molecular weight polyether polyols, a process f, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low-odor, higher molecular weight polyether polyols, a process f will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-634530

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.