ABSTRACT:
A polyester film which has the in-plane rate of dimensional change of more than 0.02%, but not more than 0.05%, when the film is kept for 72 hours under the conditions of temperature 60.degree. C. and relative humidity 80%, and the average value of the in-plane rate of dimensional change of from -0.07% to 0.03% and the in-plane anisotropy of the in-plane rate of dimensional change of from 0% to 0.08%, when the film is kept for 30 minutes at a temperature of 105.degree. C. This polyester film is low in heat shrinkage and excellent in thermal dimensional stability. A heat-development, photographic light-sensitive material using the polyester film is low in heat shrinkage and excellent in thermal dimensional stability.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Low-heat-shrinkage polyester film and heat-development photograp does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low-heat-shrinkage polyester film and heat-development photograp, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low-heat-shrinkage polyester film and heat-development photograp will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2098266

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.