ABSTRACT:
A high strength, low coefficient of thermal expansion superalloy exhibiting improved toughness over a broad temperature range down to about 4.degree. K. The composition is adapted for use with wrought superconducting sheathing.
REFERENCES:
patent: 3971677 (1976-07-01), Mason et al.
patent: 4066447 (1978-01-01), Smith, Jr. et al.
patent: 4144102 (1979-03-01), Smith, Jr. et al.
patent: 4785142 (1988-11-01), Smith, Jr. et al.
patent: 5304346 (1994-04-01), O'Donnell et al.
Hwang Il S.
Smith Darrell F.
Stein Larry I.
INCO Alloys International, Inc.
Massachusetts Institute of Technology
Steen Edward A.
Yee Deborah
LandOfFree
Low expansion superalloy with improved toughness does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low expansion superalloy with improved toughness, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low expansion superalloy with improved toughness will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1842778