ABSTRACT:
A cast iron having an austenitic matrix and consisting essentially of from 1% up to 3.5% carbon, up to 1.5% silicon, from 32% to 39.5% nickel, from 1% to less than 4% cobalt, up to 41% of the combined total of nickel plus cobalt and the balance substantially all iron provides a low expansion coefficient, good castability, good cutting properties and good damping capacity. (% is meant for % by weight)

REFERENCES:
patent: 5030299 (1991-07-01), Nishimura et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Low expansion cast iron does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low expansion cast iron, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low expansion cast iron will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-973738

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.