ABSTRACT:
Direct electric current arc welding between an electrode and a workpiece surface is accomplished in the electric current range of about 0.5-45 amps while reversing the polarities between the electrode and the workpiece surface at a low frequency rate in the range of about 1-1000 cycles per second, in a series of polarity cycles. The workpiece surface, in at least some of the cycles, is positive for a time less than that surface is negative to result in anodic cleaning of the workpiece surface. If the arc is extinguished during a polarity reversal, the arc is maintained, for example, by restriking.

REFERENCES:
patent: 3071678 (1963-01-01), Neely et al.
patent: 3591759 (1971-07-01), Stand
patent: 3598954 (1971-08-01), Iceland et al.
patent: 3781508 (1973-12-01), Dauer et al.
patent: 4125754 (1978-11-01), Wasserman et al.
patent: 4142089 (1979-02-01), Lau et al.
patent: 4472619 (1984-09-01), Ueda et al.
patent: 4621183 (1986-11-01), Takeuchi et al.
patent: 4672171 (1987-06-01), Cusimano et al.
patent: 4689463 (1987-08-01), Shubert
patent: 4739146 (1988-04-01), Lindland et al.
patent: 4745256 (1988-05-01), Shubert
patent: 4808055 (1989-02-01), Wertz et al.
patent: 4822248 (1989-04-01), Wertz et al.
patent: 4878953 (1989-11-01), Saltzman et al.
patent: 4904843 (1990-02-01), Hori et al.
patent: 4928879 (1990-05-01), Rotolico
patent: 4947021 (1990-08-01), Stava
patent: 4990739 (1991-02-01), Zaplatynsky
patent: 5021629 (1991-06-01), Shimomura
patent: 5148986 (1992-09-01), Rusch
patent: 5220151 (1993-06-01), Terayama et al.
patent: 5264679 (1993-11-01), Martin
patent: 5349159 (1994-09-01), Mita et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Low electric D.C., low time rate polarity reversing arc welding does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low electric D.C., low time rate polarity reversing arc welding , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low electric D.C., low time rate polarity reversing arc welding will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1222716

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.