ABSTRACT:
A nickel-base superalloy article for use in turbines has increased creep resistance and lower density. The superalloy article includes, as measured in % by weight, 6.0-12.0% Mo, 5.5-6.5% Al, 3.0-7.0% Ta, 0-15% Co, 2.0-6.0% Cr, 1.0-4.0% Re, 0-1.5% W, 0-1.5% Ru, 0-2.0%-Ti, 0-3.0% Nb, 0-0.2% Hf, 0-0.02% Y, 0.001-0.005% B, 0.01-0.04% C, and a remainder including nickel plus impurities.
REFERENCES:
patent: RE29920 (1979-02-01), Baldwin
patent: 4284430 (1981-08-01), Henry
patent: 4388124 (1983-06-01), Henry
patent: 4683119 (1987-07-01), Selman et al.
patent: 5077141 (1991-12-01), Naik et al.
patent: 5395584 (1995-03-01), Berger et al.
patent: 5916382 (1999-06-01), Sato et al.
patent: 6096141 (2000-08-01), King et al.
patent: 6177046 (2001-01-01), Simkovich et al.
Gabb Timothy P.
MacKay Rebecca A.
Nathal Michael V.
Smialek James L
Neal Arlene P.
Sheehan John P.
Stone Kent N.
The United States of America as Represented by the Administrator
LandOfFree
Low density, high creep resistant single crystal superalloy... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low density, high creep resistant single crystal superalloy..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low density, high creep resistant single crystal superalloy... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3847337