ABSTRACT:
A low alloy white cast iron is disclosed. The alloy consists essentially, in weight percent, of about 2.5 to 4% carbon, 0.3 to 0.8% silicon, 0.3 to 1.0% manganese, and 1.7 to 3.5% nickel, the rest being iron except for incidental impurities commonly found in cast iron. The alloy has a microstructure consisting essentially of martensite and carbide and a minimum hardness of 600 B.H.N.
REFERENCES:
patent: 3909252 (1975-09-01), Kuriyama et al.
patent: 3951650 (1976-04-01), Miyashita
Engineering Properties and Applications of Ni-Hard, 1978, The International Nickel Co., Inc.
A Dictionary of Metallurgy, A. D. Merriman, pp. 293-294.
Farge Jean C.
Fortin Robert
Noranda Mines Limited
Sheehan John P.
LandOfFree
Low alloy white cast iron does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low alloy white cast iron, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low alloy white cast iron will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2167031