ABSTRACT:
A method for producing an electrochemically advantageous lithium ion-conductive solid electrolyte with high ionic conductivity, low electronic conduction and electrochemical stability is disclosed. The method comprises the steps of synthesizing lithium sulfide by reacting lithium hydroxide with a gaseous sulfur source at a temperature of not less than 130.degree. C. and not more than 445.degree. C., thermally melting plural compounds containing at least silicon sulfide and the synthesized lithium sulfide, and cooling the molten mixture. The silicon sulfide is synthesized by the steps of adding a silicon powder to molten sulfur while stirring to disperse the silicon powder in the molten sulfur and heating the silicon powder-dispersed sulfur in a reaction chamber under reduced pressure.
REFERENCES:
patent: 3321326 (1967-05-01), Young et al.
patent: 4465746 (1984-08-01), Akridge
Ikeda Nobuhiko
Iwamoto Kazuya
Kondo Shigeo
Takada Kazunori
Uematsu Toshikatsu
Koslow Melissa
Matsushita Electric - Industrial Co., Ltd.
LandOfFree
Lithium ion-conductive solid electrolyte and method for producin does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Lithium ion-conductive solid electrolyte and method for producin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Lithium ion-conductive solid electrolyte and method for producin will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-699426