ABSTRACT:
A nickel base superalloy composition useful in the cast+HIP+heat treated condition is described. Articles having the invention composition have properties which are comparable to similarly processed IN718 articles. The invention alloys have an as-cast microstructure which is substantially free from Laves phase, even at slow solidification rates. As a result, the alloys are significantly more weldable than IN718. This desirable microstructure is achieved by modifications of the chromium, molybdenum, iron, and nickel contents compared to the typical IN718 composition.
REFERENCES:
patent: 3046108 (1962-07-01), Eiselstein
R. Vincent, "Precipitation Around Welds in the Nickel-Base Superalloy, Inconel 718", Acta Metallurgica, vol. 33, No. 7, pp. 1205-1216 (1985).
R. C. Hall, "The Metallurgy of Alloy 718," Journal of Basic Engineering, pp. 511-516 (Sep. 1967).
H. L. Eiselstein, "Metallurgy of a Columbium-Hardened Nickel-Chromium-Iron Alloy", American Society for Testing and Materials, Special Technical Publication No. 369, Advances in the Technology of Stainless Steels and Related Alloys, Philadelphia, Apr. 1965.
H. J. Wagner and A. M. Hall, "Physical Metallurgy of Alloy 718", Defense Metal Information Center Report 217, Battelle Memorial Institute, Columbus, Jun. 1, 1965.
Brown Edgar E.
Snyder Sherman M.
Dean R.
Rashid James M.
United Technologies Corporation
LandOfFree
Laves free cast+hip nickel base superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Laves free cast+hip nickel base superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Laves free cast+hip nickel base superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-503040