ABSTRACT:
A process is provided for laser welding a nickel or cobalt based superalloy article to minimize cracking by preheating the entire weld area to a ductile temperature, maintaining such temperature during welding and solidification of the weld, with the welding utilizing a powder alloy feed and the speed of the laser controlled to less than 10 inches per minute.

REFERENCES:
patent: 4804815 (1989-02-01), Everett
patent: 5106010 (1992-04-01), Stueber et al.
patent: 5374319 (1994-12-01), Stueber et al.
patent: 5554837 (1996-09-01), Goodwater et al.
patent: 5900170 (1999-05-01), Marcin, Jr. et al.
patent: 5914059 (1999-06-01), Marcin, Jr. et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Laser welding superalloy articles does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Laser welding superalloy articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Laser welding superalloy articles will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-994908

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.