ABSTRACT:
A process is described in which a structured aggregated kaolin pigment is prepared by mixing substantially dry kaolin in particulate form with an aqueous alkali metal silicate to deposit on the surface of the kaolin particles a substantially molecular level of said silicate without formation of silica gel, drying the treated kaolin without calcination and exposing it to an acidic gas. The product is useful as a pigment in the coating or filling of paper.

REFERENCES:
patent: 4299807 (1981-11-01), Angel et al.
patent: 4419228 (1983-12-01), Cook et al.
patent: 4650521 (1987-03-01), Kuppelman et al.
patent: 4738726 (1988-04-01), Pratt et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Kaolinite aggregation using sodium silicate does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Kaolinite aggregation using sodium silicate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Kaolinite aggregation using sodium silicate will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1656798

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.