ABSTRACT:
The problem of working an amorphous alloy is overcome by heating the alloy at a rate of temperature increase above about 1000.degree. C. per minute. The amorphous alloy is worked by homogeneous deformation after its temperature has been very rapidly increased to above the softening temperature of the alloy. Desirable magnetic properties of the alloy are preserved by working the alloy in this fashion and also tool life is extended.
REFERENCES:
patent: 4284441 (1981-08-01), Satoh et al.
patent: 4288260 (1981-09-01), Senno et al.
patent: 4444602 (1984-04-01), Makino et al.
patent: 4482402 (1984-11-01), Taub
patent: 4584036 (1986-04-01), Taub et al.
patent: 4596613 (1986-06-01), Lin et al.
Scaling the Kinetics of Flow and Relaxation in Amorphous Alloys; Materials Science & Engineering, 62 (1984) 249-260, by A. Taub and J. Walter.
Frischmann Peter G.
Taub Alan I.
Davis Jr. James C.
General Electric Company
Rochford Paul E.
Sheehan John P.
Webb II Paul R.
LandOfFree
Isothermal hold method of hot working of amorphous alloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Isothermal hold method of hot working of amorphous alloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Isothermal hold method of hot working of amorphous alloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-461481