ABSTRACT:
A spinodal decomposition-type hard or semi-hard magnetic alloy consisting by weight essentially of 3 to 20 % cobalt, 10 to 40 % chromium, 0.2 to 5 % one or both of niobium and tantalum, 0 to 5 % aluminum and the balance of iron. When aluminum is to be incorporated, its lower limit should be 0.5 %.
REFERENCES:
patent: 3170112 (1965-02-01), Bungardt et al.
patent: 3588764 (1971-06-01), Olsen et al.
patent: 3806336 (1974-04-01), Kaneko et al.
Dubno Herbert
Inoue-Japax Research Inc.
Ross Karl F.
Satterfield Walter R.
LandOfFree
Iron-chromium-cobalt spinodal decomposition-type magnetic alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Iron-chromium-cobalt spinodal decomposition-type magnetic alloy , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Iron-chromium-cobalt spinodal decomposition-type magnetic alloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-676074