The strength of interstitial free steels is increased by up to 100% and the ductile to brittle transition temperature is decreased by up to 100.degree. C. by warm finish rolling in the single phase ferrite region below A.sub.rl to effect ferrite dynamic recrystallization of the steel microstructure to a ferrite structure of grain size having a grain size of up to 5 .mu.m, and especially an ultra fine grain size of 1 to 2 .mu.m; the method may be employed in various hot working methods including strip and rod mills, planetary hot rolling and extrusion.

REFERENCES:
patent: 3755004 (1973-08-01), Miller
patent: 4466842 (1984-08-01), Yada et al.
patent: 4720307 (1988-01-01), Matsumoto et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Interstitial free steels and method thereof does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Interstitial free steels and method thereof, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Interstitial free steels and method thereof will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-533222

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.