ABSTRACT:
A rosin based intermediate softening point (ISPR) tackifier has a ring and ball softening point of from 35 to 60° C. A hot-melt pressure-sensitive adhesive (HMPSA) composition contains an elastomeric component, such as a blend of SIS and SB block copolymers, and a tackifying component comprising one or more rosin based ISPRs having a ring and ball softening point of from 35 to 60° C.

REFERENCES:
patent: 3577398 (1971-05-01), Pace et al.
patent: 3692756 (1972-09-01), St. Cyr
patent: 4797460 (1989-01-01), Davis
patent: 5041492 (1991-08-01), Koprowicz et al.
patent: 5412032 (1995-05-01), Hansen et al.
patent: 5428109 (1995-06-01), Kuroiwa et al.
patent: 5532306 (1996-07-01), Kauffman et al.
patent: 5853874 (1998-12-01), Jacob
patent: 6214935 (2001-04-01), Sasaki et al.
patent: 6218457 (2001-04-01), Fralich et al.
patent: 6340236 (2002-01-01), Hisanaga
patent: 6455168 (2002-09-01), Kuno et al.
patent: 2004/0167258 (2004-08-01), Drogou et al.
patent: 2004/0229000 (2004-11-01), Khandpur et al.
patent: 2005/0075431 (2005-04-01), Haner et al.
patent: 0 259 697 (1988-03-01), None
patent: 1 447 419 (1976-08-01), None
patent: 00/04108 (2000-01-01), None
patent: 00/78886 (2000-12-01), None
International Search Report for corresponding PCT/US2006/028781 mailed Nov. 16, 2006.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Intermediate softening point resin-based hot melt PSAs does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Intermediate softening point resin-based hot melt PSAs, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Intermediate softening point resin-based hot melt PSAs will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4178061

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.