ABSTRACT:
A process and apparatus is provided for laser welding a nickel and/or cobalt based superalloy article comprising: preheating the entire weld area and adjacent region to a ductile temperature with an induction heat coil and maintaining such temperature during welding and solidification of the weld; and welding the preheated article utilizing a laser with a powder alloy feed with a control means controlling the laser, power feed and motion system on which the article is fixtured, wherein the control means includes a vision system which digitizes the weld area providing a path for the laser welding to follow.
REFERENCES:
patent: 3246392 (1966-04-01), Altgelt
patent: 3535768 (1970-10-01), Pruitt et al.
patent: 3619547 (1971-11-01), Cavagnero
patent: 3660882 (1972-05-01), Widowitz et al.
patent: 4402447 (1983-09-01), Przybyszewski et al.
patent: 4498617 (1985-02-01), Guertin et al.
patent: 4576874 (1986-03-01), Spengler et al.
patent: 4611744 (1986-09-01), Fraser et al.
patent: 4613744 (1986-09-01), Fraser et al.
patent: 4675204 (1987-06-01), Nicoll et al.
patent: 4675502 (1987-06-01), Haefner et al.
patent: 4733049 (1988-03-01), Lemelson
patent: 4737613 (1988-04-01), Frye
patent: 4804815 (1989-02-01), Everett
patent: 4918805 (1990-04-01), Liszka et al.
patent: 4998005 (1991-03-01), Rathi et al.
patent: 5106010 (1992-04-01), Stueber et al.
patent: 5160822 (1992-11-01), Aleshin
patent: 5168141 (1992-12-01), Tashjian et al.
patent: 5208431 (1993-05-01), Uchiyama et al.
patent: 5224997 (1993-07-01), Grilloud et al.
patent: 5225247 (1993-07-01), Dotsch et al.
patent: 5229571 (1993-07-01), Neiheisel
"Blade Repair Time Cut In Half", Oct. 1992, Industrial Laser Review, 11, 13.
"CNC Laser System", Multi Axis CNC Laser System, 5 Axis CNC Laser System, S. E. Huffman Corp., 1050 Huffman Way, Clover, SC 29710, published prior Sep. 3, 1993.
Welding Handbook, Seventh Edition, vol. 4 Metals And Their Weldability, W. H. Kearns, Editor, 1982 pp. 232-237.
Doyle Brian G.
Goodwater Frank
Huynh Lang D.
Kang David S.
Li Hon
Bittman Mitchell D.
Chromalloy Gas Turbine Corporation
Mills Gregory L.
Walberg Teresa J.
LandOfFree
Interactive laser welding at elevated temperatures of superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Interactive laser welding at elevated temperatures of superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Interactive laser welding at elevated temperatures of superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1322468