ABSTRACT:
A method for inhibiting stress-corrosion cracking of a steel pipeline transmitting gas under elevated pressure provided with an external protective coating and means for cathodic protection, and steep pipe and pipelines so protected are described. The method consists of introducing a composition containing at least one of the inhibitors, calcium monobasic phosphate, sodium monobasic phosphate, sodium tripolyphosphate and potassium silicate, into a buried pipeline environment. The inhibiting composition may be simply introduced to the environment adjacent the pipeline or it may be incorporated in a coating on the pipeline, either in the primer or in a top coating thereover or in an intermediate coating between a conventional primer and topcoating, or in a tape applied to the pipeline.

REFERENCES:
patent: 2685523 (1954-08-01), Cross et al.
patent: 2861892 (1958-11-01), Radd et al.
patent: 2883289 (1959-04-01), Furey et al.
patent: 3070065 (1962-12-01), Hill
patent: 3333973 (1967-08-01), Freiman
patent: 3354169 (1967-11-01), Shafer et al.
patent: 3357927 (1967-12-01), Marsh et al.
patent: 3468687 (1969-09-01), Thomas
patent: 3689305 (1972-09-01), Hausmann
fraser, Corrosion Control in Idle Pipelines, Materials Performance, Mar. 1974, pp. 29-30.
Holzworth et al., Inhibition of Stress Corrosion in Type 304 Stainless Steel by Lithium Silicate, Corrosion-Nace, vol. 25, No. 7, July 1969, pp. 287-288.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Inhibition of stress-corrosion cracking of steel pipeline does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Inhibition of stress-corrosion cracking of steel pipeline, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Inhibition of stress-corrosion cracking of steel pipeline will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1930407

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.