ABSTRACT:
This invention relates to a process of inhibiting pitting corrosion which is characterized by the use of synergistic mixtures of organic anodic and cathodic corrosion inhibitors. These synergistic mixtures effectively inhibit pitting corrosion in highly oxygenated systems without the conventional use of heavy metals such as zinc (Zn) or chromium (Cr). This invention also relates to the use of alkoxysilyl alkylene polyamines as pitting corrosion inhibitors.

REFERENCES:
patent: 3716569 (1973-02-01), Redmore et al.
patent: 3803047 (1974-04-01), Hwa
patent: 3816184 (1974-06-01), Redmore et al.
patent: 4014814 (1977-03-01), Zecher
patent: 4033896 (1977-07-01), Mitchell et al.
patent: 4072626 (1978-02-01), Finney
patent: 4134959 (1979-01-01), Merke et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Inhibition of pitting corrosion does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Inhibition of pitting corrosion, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Inhibition of pitting corrosion will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2241411

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.