ABSTRACT:
A mold structure for casting large metallic parts such as ingots so as to avoid the formation of the "shrinkage pipe" which normally develops on the exposed top surface of such castings during their solidification comprises a cap for placement on a mold which includes a diaphragm having a front surface located to intercept radiation emitted from the top surface of the cooling metal mass and to re-emit radiation back thereto, and a reflector for returning radiation emitted from the back surface of the diaphragm such as an infrared reflector or a stack of baffles. The cap may include a cooler for cooling the reflective surface and suitable ports which allow the interior of the mold and cap to be evacuated. Portions of the mold adjacent its open top may be provided with insulation to prevent heat loss from the metal by conduction. A heater for providing make-up heat to the top surface of the metal mass may also be included in the structure.
REFERENCES:
patent: 3012296 (1961-12-01), Wiesner
patent: 4050668 (1977-09-01), Perri
Batten, Jr. J. Reed
Godici Nicholas P.
Pyreflex Corp.
LandOfFree
Inhibiting shrinkage pipe formation of metal casting does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Inhibiting shrinkage pipe formation of metal casting, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Inhibiting shrinkage pipe formation of metal casting will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-599798