ABSTRACT:
Alumina slurries (suspensions) can be stabilized against viscosity increases by treating with water which has been heated to temperatures of from about 40.degree. C. to about 100.degree. C., then cooling, decanting the water, and recovering a wet cake. Water is then added to the recovered wet cake alumina to obtain a slurry with a desired alumina content and CO.sub.2 is sparged through the finished slurry. Optionally, hot water saturated with carbon dioxide can be used for the treatment, to extend the stability of the slurry. Peptizing agents can be used as usual.
REFERENCES:
patent: 3653937 (1972-04-01), Koenig
patent: 4117105 (1978-09-01), Hertzenberg et al.
Carter Herbert T.
Conoco Inc.
Schupbach, Jr. Cortlan R.
LandOfFree
Increasing alumina slurry life does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Increasing alumina slurry life, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Increasing alumina slurry life will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2039918