ABSTRACT:
The impact strength of a thermoplastic molding composition containing aromatic polycarbonate resin and a copolymer is improved upon the incorporation therewith of a particular silicone rubber powder. The silicone rubber powder, added at a level of about 3 to 25 percent, contains a mixture of (a) a polydiorganosiloxane and (b) finely divided silica filler.
REFERENCES:
patent: 3751519 (1973-08-01), Bostick et al.
patent: 4197384 (1980-04-01), Bialous et al.
patent: 5153238 (1992-10-01), Bilgrien et al.
patent: 5322882 (1994-06-01), Okamoto
R. Buch et al, "Silicone-Based Additives for Thermoplstic Resins Providing improved Impact Strength, Processing and Fire Retardant Synergy", (Dow Corning Corp)--Fire Retardant Chem. Assoc, Oct. 26-29, 1993.
Mason James P.
White Roger J.
Bayer Corporation
Gil Joseph C.
Preis Aron
Warzel Mark L.
LandOfFree
Impact modified thermoplastic molding composition does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Impact modified thermoplastic molding composition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Impact modified thermoplastic molding composition will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-140201