Impact modification of polypropylene with styrene/isoprene tetra

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

528 89, C08L 5302

Patent

active

054929679

ABSTRACT:
Compositions consisting essentially of from 60% to 95% by weight of the polymer components of a high flow polypropylene and from 40% to 5% by weight of a polystyrene-hydrogenated polyisoprene-polystyrene-hydrogenated polyisoprene block copolymer have excellent low temperature impact strength and high heat distortion temperature for molding large automobile parts.

REFERENCES:
patent: 4904731 (1990-02-01), Holden
patent: 5045589 (1991-09-01), Ueno

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Impact modification of polypropylene with styrene/isoprene tetra does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Impact modification of polypropylene with styrene/isoprene tetra, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Impact modification of polypropylene with styrene/isoprene tetra will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1356580

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.