ABSTRACT:
The recovery of metal values such as nickel from a metal bearing source such as lateritic ores in which the metal bearing source is subjected to a reductive roast at an elevated temperature in the range of from about 700.degree. to about 1300.degree. F. in contact with at least one additive and thereafter extracting the metal bearing source in an ammoniacal solution whereby the desired metal such as nickel is leached out and recovered, the yield of the desired metal may be increased by subjecting the source to an annealing process during the reductive roast thereof.

REFERENCES:
patent: 3100700 (1963-08-01), Hills
patent: 3655364 (1972-04-01), Evans et al.
patent: 3772423 (1973-11-01), Stevens et al.
patent: 3772424 (1973-11-01), Stevens et al.
patent: 3845189 (1974-10-01), Miller et al.
patent: 3860689 (1975-01-01), Setton et al.
patent: 3985556 (1976-10-01), Siemens et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Hydrometallurgical recovery of nickel values does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Hydrometallurgical recovery of nickel values, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Hydrometallurgical recovery of nickel values will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2021163

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.