ABSTRACT:
A two-part sizing composition that imparts improved resistance to hydrolysis of reinforced composites including a size composition and a binder composition is provided. The size composition may include one or more coupling agents, one or more lubricants, and at least one wetting agent. The binder composition may include a copolymer formed from maleic anhydride and at least one other copolymerizable monomer, at least one crosslinking agent, and a surfactant or mixture of surfactants. In at least one exemplary embodiment, the maleic anhydride copolymer is a maleic anhydride-butadiene copolymer partial ammonium salt. The size composition may be applied to a reinforcing fiber material before the binder size material is applied. The two-part size composition may be applied to a reinforcing fiber material to form a reinforcing fiber product which may then be densified or compacted to form a densified reinforcing fiber product, such as a pellet.

REFERENCES:
patent: 3414432 (1968-12-01), Mertzweiller et al.
patent: 3816235 (1974-06-01), Lin
patent: 4609591 (1986-09-01), Pollet et al.
patent: 5324755 (1994-06-01), Kilius et al.
patent: 5578535 (1996-11-01), Hill et al.
patent: 5693378 (1997-12-01), Hill et al.
patent: 5811480 (1998-09-01), Kirchmeyer et al.
patent: 5868982 (1999-02-01), Strait et al.
patent: 5945134 (1999-08-01), Strait et al.
patent: 5972503 (1999-10-01), Woodside
patent: 6365090 (2002-04-01), Strait et al.
patent: 6365272 (2002-04-01), Masson et al.
patent: 6407157 (2002-06-01), Oyamada et al.
patent: 6659756 (2003-12-01), Strait et al.
patent: 2003/0176565 (2003-09-01), Piret et al.
patent: 60-44535 (1985-03-01), None
patent: 60044535 (1985-03-01), None
patent: 3-80135 (1991-04-01), None
patent: 2003201671 (2003-07-01), None
JP 3-80135 Abstract in English.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Hydrolization resistant sizing composition does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Hydrolization resistant sizing composition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Hydrolization resistant sizing composition will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3688119

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.