Hot isostatic pressing of single crystal superalloy articles

Metal treatment – Process of modifying or maintaining internal physical... – Processes of coating utilizing a reactive composition which...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148675, C21D 178

Patent

active

055736092

ABSTRACT:
A method for the densification of a shaped nickel base single crystal alloy article utilizing a pre-HIP, a hot isostatic pressing (HIP) step, and post-HIP solution heat treatment to enhance removal of casting porosity in a finished article.

REFERENCES:
patent: 3567526 (1971-03-01), Gell et al.
patent: 4116723 (1978-09-01), Gell et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4222794 (1980-09-01), Schweizer et al.
patent: 4345950 (1982-08-01), O'Hara
patent: 4528048 (1985-07-01), Gell et al.
patent: 4529452 (1985-07-01), Walker
patent: 4597809 (1986-07-01), Duhl et al.
patent: 4605452 (1986-08-01), Gemma et al.
patent: 4743312 (1988-05-01), Eridon et al.
patent: 4981528 (1991-01-01), Fritzemeier et al.
Evans, D. J., "Powder Metallurgy Processing of High Strength Turbine Disk Alloys," American Society of Mechanical Engineers, Mar. 1976, Pub. 76-GT-96.
Van Drunen, G. et al, "Hot Isostatic Processing of IN-738 Turbine Blades", Westinghouse Canada Limited 13-1/11, no date.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Hot isostatic pressing of single crystal superalloy articles does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Hot isostatic pressing of single crystal superalloy articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Hot isostatic pressing of single crystal superalloy articles will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-559551

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.