ABSTRACT:
An improved austenitic alloy having in wt % 19-21 Cr, 30-35 Ni, 1.5-2.5 Mn, 2-3 Mo, 0.1-0.4 Si, 0.3-0.5 Ti, 0.1-0.3 Nb, 0.1-0.5 V, 0.001-0.005 P, 0.08-0.12 C, 0.01-0.03 N, 0.005-0.01 B and the balance iron that is further improved by annealing for up to 1 hour at 1150.degree.-1200.degree. C. and then cold deforming 5-15 %. The alloy exhibits dramatically improved creep rupture resistance and ductility at 700.degree. C.
REFERENCES:
Swindeman et al, "Procurement and Screening Test Data for Advanced Austenitic Alloys for 650.degree. C. Steam Service," ORNL/TM-10206/P1.
Goodwin Gene M.
Maziasz Philip J.
Swindeman Robert W.
Hamel Stephen D.
Hightower Judson R.
Lovingood Katherine P.
Rutledge L. Dewayne
Schumaker David
LandOfFree
High temperature creep resistant austenitic alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with High temperature creep resistant austenitic alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High temperature creep resistant austenitic alloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-170293