Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – From boron reactant having at least one boron to hydrogen or...
Patent
1977-02-22
1979-03-20
Marquis, Melvyn I.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
From boron reactant having at least one boron to hydrogen or...
260 37SB, 528 30, 528 32, 528 34, 528 41, 528 43, C08G 7704
Patent
active
041455045
ABSTRACT:
Carborane-siloxane polymers are conveniently prepared by the polymerization of a carborane disilanol and either a silyl diamine, a ureido-silane, or a silyl dicarbamate. The resulting linear polymers are characterized by relatively high molecular weights and are elastomeric in nature. These gumstocks are compounded with suitable fillers and additives and fabricated into cured elastomeric articles. The carborane-siloxane elastomers exhibit excellent high temperature properties which render them especially useful for a wide variety of applications, such as gaskets, seals, wire and cable insulation and the like.
REFERENCES:
patent: 3388092 (1968-06-01), Heying et al.
patent: 3661847 (1972-05-01), Chapman
patent: 3733298 (1973-05-01), Knollmueller
Hedaya Eddie
Kawakami James H.
Kwiatkowski George T.
Marquis Melvyn I.
Moran William Raymond
Union Carbide Corporation
LandOfFree
High temperature carborane-siloxane elastomers intermediate poly does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with High temperature carborane-siloxane elastomers intermediate poly, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High temperature carborane-siloxane elastomers intermediate poly will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-221814