Metal treatment – Compositions – Heat treating
Patent
1987-05-21
1989-03-21
Dean, R.
Metal treatment
Compositions
Heat treating
148 3, 148 115N, 148 127N, 148162, 148410, 148428, C22F 110
Patent
active
048140236
ABSTRACT:
A novel alloy is provided having approximately the following ingredient formula:
REFERENCES:
patent: 4685977 (1987-08-01), Chang
Davis Jr. James C.
Dean R.
General Electric Company
Magee Jr. James
Rochford Paul E.
LandOfFree
High strength superalloy for high temperature applications does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with High strength superalloy for high temperature applications, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High strength superalloy for high temperature applications will most certainly appreciate the feedback.