ABSTRACT:
A process for preparing a consolidated nickel-base superalloy compact suitable for tensile force inducing high strain rate deformation. It includes the steps of: preparing a melt of a nickel-base superalloy in a vacuum; atomizing the melt into powder in a protective atmosphere; collecting the powder; screening the powder to proper size; introducing the powder into a container; evacuating and sealing the container in a vacuum; and consolidating the powder under pressure at a temperature below the solidus temperature of the alloy and at a temperature at which grain boundaries grow past prior particle boundaries.
REFERENCES:
patent: 3639179 (1972-02-01), Reichman et al.
patent: 3975219 (1976-08-01), Allen et al.
patent: 4226644 (1980-10-01), Cox et al.
patent: 4439236 (1984-03-01), Ray
patent: 4576653 (1986-03-01), Ray
patent: 4717435 (1988-01-01), Kawasaki et al.
patent: 4886639 (1989-12-01), Andrees et al.
patent: 5009704 (1991-04-01), Banik
patent: 5100616 (1992-03-01), Kawasaki et al.
Dropkin Robert F.
Mai Ngoclan
Special Metals Corporation
LandOfFree
High strain rate deformation of nickel-base superalloy compact does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with High strain rate deformation of nickel-base superalloy compact, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High strain rate deformation of nickel-base superalloy compact will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1825470