ABSTRACT:
Using a combination of relatively coarse filler and latex binder, a very high solids coating (about 85% or higher) can be produced with a relatively low working viscosity. These very high solids coatings can be applied in thick single layers and oven cured without cracking. They maintain more than 80% of their original wet thickness. The resulting coating provides an extremely hard and durable surface, even on relatively soft mineral fiber board ceiling tiles or wall panels.

REFERENCES:
patent: 2411470 (1946-11-01), Patton
patent: 4559377 (1985-12-01), Gleason et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

High solids, low shrinkage coating does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with High solids, low shrinkage coating, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High solids, low shrinkage coating will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1947182

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.