ABSTRACT:
A high temperature oxidation and corrosion resistant coated nickel-base superalloy article comprising (a) a nickel-base superalloy article, and [(b) a first] adjacent thereto (b) a CoCrAl(Y) coating having a substantially uniform composition [consisting essentially] composed of, on a weight basis, approximately 26-32% chromium, 3-9% aluminum, 0-1% yttrium, the rare earth elements, platinum or rhodium, and the balance [nickel] cobalt and impurities ordinarily associated with the aforementioned constituents.
REFERENCES:
patent: 3676085 (1972-07-01), Evans et al.
patent: 3873347 (1975-03-01), Walker et al.
patent: 3918139 (1975-11-01), Felten
patent: 3928026 (1975-12-01), Hecht et al.
patent: 3957454 (1976-05-01), Bessen
patent: 3976436 (1976-08-01), Chang
patent: 3978251 (1976-08-01), Stetson
patent: 3993454 (1976-11-01), Giggins, Jr. et al.
patent: 3998603 (1976-12-01), Rairden
patent: 4005989 (1977-02-01), Preston
patent: 4018569 (1977-04-01), Chang
patent: 4022587 (1977-05-01), Wlodek
patent: 4034142 (1977-07-01), Hecht
patent: 4101713 (1978-07-01), Hirsh et al.
patent: 4144380 (1979-03-01), Beltran et al.
Wolf, P. C., "Vacuum Plasma Spray Process and Coatings", Trans. 9th Int. Thermal Spraying Conf., pp. 187-196, (1980).
Smith, R. W., et al., "Low Pressure Plasma Spray Coatings for Hot Corrossion Resistance", Trans. 9th Int. Thermal Spraying Conf., pp. 334-343, (1980).
Powell, C. F., et al., Vapor Deposition, John Wiley & Sons, Inc., pp. 242-246, (1966).
Kennedy, K., "Alloy Deposition from Single and Multiple Electron Beam Evaporation Sources", AVS 1968 Regional Symposia, pp. 1-8.
Messbacher, A., et al., "Vacuum Plasma Spraying of Protective Hot Gas Corrossion Coatings", Trans. 8th Int. Thermal Spray Conf. Amer. Weld Soc., pp. 25-37, (1976).
Rairden, J. R., et al., "The 3rd Conference on Gas Turbine Materials in a Marine Environment Coatings for Directional Eutectics", pp. 1-11, (9/76).
Rairden, J. R., et al., "Coatings for Protecting Nickel-Base TaC Eutectics Against Oxidation", Thin Solid Films, vol. 40, pp. 291-298, (1977).
Boone, D. H., et al., "Electron Beam Evaporation . . . ", Thin Solid Films, vol. 64, pp. 299-304, (1979).
Talboom, F. P., et al., Evaluation of Advanced Superalloy Protection Systems, NASA CR-72813 PWA-4055, pp. 1-9, 24, 46-56, (1970).
Foster, J. S., et al., "Vacuum Deposition of Alloys-Theoretical and Practical Considerations", J. Vac. Sci., vol. 9, pp. 1379-1381, 1384, (1972).
Nimmagadda, R., et al., "Preparation of Alloy by Continuous Electron Beam Evaporation from a Single Rod-Fed Source", J. Vac. Sci. Tech., vol. 9, (1972).
Boone, D. H., et al., "Some Effects of Structure . . . ", J. Vac. Sci. Technol., vol. 11, pp. 641-646, (1974).
Rairden, J. R., et al., Coatings for Directional Eutectics, The 3rd Conf. on Gas Turbines in a Marine Environment Paper 4, pp. 1-11, (9/76).
Rairden, J. R., et al., Coatings for Directional Eutectics, NASA CR-135050, NAS 3-17815, pp. 1-73 and D-1 to ll, (7/25/76).
Jackson, M. R., et al., Coatings for Directional Eutectics, NASA SRD-74-047, NASA CR-134665, pp. 1-87, D1-12, (1/74).
Davis Jr. James C.
General Electric Company
Lewis Michael L.
MaLossi Leo I.
LandOfFree
High integrity CoCrAl(Y) coated nickel-base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with High integrity CoCrAl(Y) coated nickel-base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High integrity CoCrAl(Y) coated nickel-base superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-198130