ABSTRACT:
A high dielectric porcelain composition having, as a main component, a Pb(Mg 1/3, Nb 2/3)O.sub.3 -PbTiO.sub.3 -Pb(Mn 1/3, Nb 2/3)O.sub.3 system including 95 mol. % of Pb(Mg 1/3, Nb 2/3)O.sub.3, 5 mol. % of PbTiO.sub.3 and 0.5 weight % of Pb(Mn 1/3, Nb 2/3)O.sub.3, and, in addition, a sub-component including PbO and ZnO. Such a dielectric porcelain is capable of being sintered at a temperature lower than 1000.degree. C. A method of reducing the sintering temperature of such a high dielectric porcelain composition, is also provided.

REFERENCES:
patent: 4265668 (1981-05-01), Fujiwara et al.
patent: 4339544 (1982-07-01), Sakabe et al.
patent: 4482935 (1984-11-01), Wheeler
patent: 4530031 (1985-07-01), Donohue

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

High dielectric porcelain composition and method of reducing sin does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with High dielectric porcelain composition and method of reducing sin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High dielectric porcelain composition and method of reducing sin will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2158237

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.