Stock material or miscellaneous articles – Web or sheet containing structurally defined element or... – Including a second component containing structurally defined...
Patent
1996-10-18
1998-05-12
Resan, Stevan A.
Stock material or miscellaneous articles
Web or sheet containing structurally defined element or...
Including a second component containing structurally defined...
428329, 428336, 428402, 428403, 428694BA, 428694BS, 428900, 423633, 106304, G11B 5708
Patent
active
057502501
ABSTRACT:
Hematite particles for a non-magnetic undercoat layer for a magnetic recording medium, comprise: high-density acicular hematite particles having an average major axial diameter of not more than 0.3 .mu.m, a major axial diameter distribution in geometrical standard of not more than 1.50 and a BET specific surface area of not less than 35 m.sup.2 /g, showing a pH of not less than 8, and containing not more than 300 ppm of soluble sodium salt, calculated as Na, and not more than 150 ppm of soluble sulfate, calculated as SO.sub.4.
REFERENCES:
patent: 5489466 (1996-02-01), Inaba et al.
patent: 5496622 (1996-03-01), Isobe et al.
patent: 5587232 (1996-12-01), Hayashi et al.
patent: 5604015 (1997-02-01), Hayashi et al.
Hayashi Kazuyuki
Iwasaki Keisuke
Morii Hiroko
Tanaka Yasuyuki
Resan Stevan A.
Toda Kogyo Corporation
LandOfFree
Hematite particles and magnetic recording medium having a non-ma does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Hematite particles and magnetic recording medium having a non-ma, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Hematite particles and magnetic recording medium having a non-ma will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-977685