ABSTRACT:
A method of increasing intergranular stress corrosion cracking resistance of Alloy 718 in water reactor environments is disclosed. The Alloy is heat treated at a high annealing temperature to dissolve .delta. precipitates. The absence of .delta. particles at the grain boundaries increases the elemental homogeneity at the boundaries and increases intergranular stress corrosion cracking resistance. In addition, the absence of .delta. phase at the grain boundaries decreases the crack propagation rate.
REFERENCES:
patent: 3046108 (1962-07-01), Eiselstein
patent: 3972752 (1976-08-01), Honnorat et al.
James, L. A. and Mills, W. J., "Effect of Heat Treatment and Heat-to-Heat Variations in the Fatigue Crack Growth Response of Alloy 718", Hanford Engineering Development Laboratory, HEDL-TME 80-9, UC-79, b, h, Apr. 1980, Part 1 & HEDL-TME 80-10, UC-79, b, h, Part 2.
Mills, W. J., "Effect of Heat Treatment on the Tensile and Fracture Toughness Behavior of Alloy 718 Weldments", Supp. to the Welding Journal, Aug. 1984, pp. 237s-245s.
Korth, Gary, "Mechanical Properties Test Data of Alloy 718 for Liquid Metal Fast Breeder Reactor Applications", Dept. of Energy, DOE Contract No. DE-AC07-761D01570, Jan. 1983.
Smolik, G. R. and Korth, G. E., "Reference Heat of Alloy 718 for Department of Energy Programs", Report TREE-1253, EG & G Idaho Inc., Apr. 1978.
Kimmmerle, W. L., Miglin, M. T., and J. L. Nelson, "Stress Corrosion Cracking of Alloy 718 in Pressurized-Water-Reactor Primary Water", Superalloy 718, ed. E. A. Loria, AIME, presented at International Symposium of Superalloy 718, Pittsburgh, Pa., Jun. 11-14, 1989.
Miglin, M. T. and Nelson, J. L., Strain Rate Sensitivity of Alloy 718 Stress Corrosion Cracking, Fontevraud II Conference Proceedings, Chinon, France, Sep. 10-14, 1990.
Kimmerle William L.
Miglin Marie T.
Dean R.
Edwards Robert J.
Kalka Daniel S.
Matas Vytas R.
Phipps Margery S.
LandOfFree
Heat treatment of Alloy 718 for improved stress corrosion cracki does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Heat treatment of Alloy 718 for improved stress corrosion cracki, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Heat treatment of Alloy 718 for improved stress corrosion cracki will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-537797