ABSTRACT:
A cobalt-free nickel-base superalloy composed of in weight % 15 Cr-5 Mo-3.5 Ti-4 Al-0.07 (max) C-remainder Ni is given a modified heat treatment. With this heat treatment the cobalt-free alloy achieves certain of the mechanical properties of the corresponding cobalt-containing nickel-base superalloy at 1200.degree. F. (650.degree. C.). Thus strategic cobalt can be replaced with nickel in the superalloy.

REFERENCES:
patent: 2570194 (1951-10-01), Bieber et al.
patent: 3272666 (1966-09-01), Symonds
patent: 3536542 (1970-10-01), Murphy et al.
patent: 4161412 (1979-07-01), Henry

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Heat treatment for superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Heat treatment for superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Heat treatment for superalloy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-446063

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.