ABSTRACT:
Heat treatments are described for improving the fatigue properties of superalloy articles, without adversely affecting other mechanical properties. The entire heat treatment process is performed below the gamma prime solvus temperature so that significant grain growth does not occur. The heat treatment cycle causes the formation of gamma prime particles in a controlled manner and morphology, first at the grain boundaries and then within the grains. The resultant microstructure possesses the benefits of a fine grain structure (improved resistance to fatigue crack initiation) and fine gamma prime particle size (improved resistance to crack growth).
REFERENCES:
patent: 4608094 (1986-08-01), Miller et al.
Blackburn Martin J.
Caless Robert H.
D'Orvilliers Anne L.
Paulonis Daniel F.
Dean R.
Sohl Charles E.
United Technologies Corporation
LandOfFree
Heat treatment for improving fatigue properties of superalloy ar does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Heat treatment for improving fatigue properties of superalloy ar, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Heat treatment for improving fatigue properties of superalloy ar will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-664771