Metal treatment – Compositions – Heat treating
Patent
1978-06-12
1980-10-07
Rutledge, L. Dewayne
Metal treatment
Compositions
Heat treating
75177, 148133, C21D 102, C22D 1600
Patent
active
042266475
ABSTRACT:
High tensile strength, creep and corrosion resistant zirconium alloys containing 7.0-10.0 wt % aluminum, 0-3 wt % in total of one or more elements selected from the group consisting of magnesium, tin, chromium, iron, carbon, silicon, yttrium, niobium, molybdenum and beryllium, the balance zirconium and incidental impurities, are produced by annealing cast alloys at a temperature below about 992.degree. C. for a period of time sufficient to produce alloys having a substantially continuous matrix of the ordered intermetallic compound Zr.sub.3 Al. The alloys may initially be hot worked at temperatures about 1000.degree. C., while in the .beta.Zr-Zr.sub.2 Al two phase region, prior to annealing. Preferred alloys contain 7.5-9.5 wt % aluminum, the balance zirconium and incidental impurities.
REFERENCES:
patent: 3125446 (1964-03-01), Johnson et al.
patent: 4000013 (1976-12-01), MacEwen et al.
patent: 4094706 (1978-06-01), Schulson et al.
Cameron Donald J.
Schulson Erland M.
Atomic Energy of Canada Limited
McClenahan W. John
Rutledge L. Dewayne
Skiff Peter K.
LandOfFree
Heat-treated zirconium alloy product does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Heat-treated zirconium alloy product, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Heat-treated zirconium alloy product will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-617058